V. S. KOPAN’, N. V .KHUTORYANS’KA, and Yu. V. KOPAN’
«Thermoelectric Absorption Effect in Carbon Nanotubes Powder»
177–184 (2010)

PACS numbers: 62.23.Pq, 72.20.Pa, 72.80.Rj, 72.80.Tm, 81.05.ub, 81.07.Wx, 85.85.+j

The difference ET between the thermoelectric power (TEP) of dry carbon nanotubes powder (CNTP) and TEP of CNTP after liquids adsorption is measured within the temperature range from 293 K to 333 K. The ET is decreasing in the series of liquids: alcohol, white spirit, water. The ET???0 in CNTP, and ET???0 in graphite powder. The ET arises owing to adsorption and tunnelling of charges across gaps between the powder particles.