Скачать полную версию статьи (в PDF формате)
В. К. Сабокарь, И. К. Петриченко, С. В. Ахонин
«Прессовая сварка алюминида титана с применением наноструктурированных прослоек»
361–367 (2012)
PACS numbers: 06.60.Vz, 62.20.Qp, 62.23.Pq, 81.20.Ev, 81.20.Vj, 81.40.Ef, 81.70.Jb
Joining of titanium aluminide of the Ti–Al–Cr system by pressure welding using nanostructured laminated interlayers at a temperature of 700?C, pressure of 200 MPa and time of 15 min is considered. Metallographic examinations and x-ray spectral microanalysis are carried out. As revealed, the annealing of a welded joint at 1260?C for 10 h provides diffusion of elements of the interlayer into the near-contact volumes of metals being joined as well as levelling of structure of the welded joints.
|